Ampicillin was obtained from Wako Pure Chemical Industries Ltd (Osaka, Japan). Anhydrotetracycline and Strep-Tactin-Sepharose were purchased from IBA. Triton X-100, ethylenediaminetetraacetic acid (EDTA), urea, l-arginine hydrochloride, l-cystine dihydrochloride, l-cysteine, bovine serum albumin (BSA), Tween 20 and 5, 5′-dithiobis-2-nitrobenzoic acid (DTNB) were obtained from Wako Pure Chemical Industries Ltd. Desthiobiotin and Orlistat were purchased from Sigma-Aldrich (Saint Louis, MO). Phenylmethylsulfonyl fluoride (PMSF) was purchased from Nacalai Tesque, Inc. (Kyoto, Japan). Rabbit anti-HPL polyclonal IgGs and anti-Strep-tag II (ST II) monoclonal IgG were obtained from Abcam (Cambridge, UK) and IBA GmbH (Gottingen, Germany), respectively. Horseradish peroxidase (HRP)-conjugated goat anti-rabbit IgG and anti-mouse IgG antibodies were from Kirkegaard and Perry Laboratories (Washington, DC, USA). Tributyrin was purchased from Wako Pure Chemical Industries Ltd (Osaka, Japan). Porcine colipase was from AbD Serotec (Kidlington, UK). Gel-filtraion FPLC columns, HiPrep 16/60 Sephacryl S-200 HR were purchased from GE Healthcare.
+ Open protocol
+ Expand
2

Silver Paste Composition Preparation

Check if the same lab product or an alternative is used in the 5 most similar protocols

Example 4

As the silver particles, AgC239 (FUKUDA METAL FOIL & POWDER Co., Ltd.) was used. As the solvent, tributyrin (boiling point 305° C., Wako Pure Chemical Industries, Ltd.), butyl stearate (boiling point 343° C., Wako Pure Chemical Industries, Ltd.), and stearic acid (boiling point 376° C., Wako Pure Chemical Industries, Ltd.) were used. The silver particles and the solvent were kneaded for 15 minutes with a stone mill at the blending ratio shown in Table 1 to manufacture a silver paste composition. The properties of this silver paste composition were measured to obtain the result shown in Table 1.

+ Open protocol
+ Expand
3

Silver Paste Composition Formulation

Check if the same lab product or an alternative is used in the 5 most similar protocols

Example 5

As the silver particles, K-0082P (METALOR) was used. As the solvent, tributyrin (boiling point 305° C., Wako Pure Chemical Industries, Ltd.), butyl stearate (boiling point 343° C., Wako Pure Chemical Industries, Ltd.), and stearic acid (boiling point 376° C., Wako Pure Chemical Industries, Ltd.) were used. The silver particles and the solvent were kneaded for 15 minutes with a stone mill at the blending ratio shown in Table 1 to manufacture a silver paste composition. The properties of this silver paste composition were measured to obtain the result shown in Table 1.

+ Open protocol
+ Expand
4

Silver Paste Composition Preparation

Check if the same lab product or an alternative is used in the 5 most similar protocols

Example 3

As the silver particles, AgC239 (FUKUDA METAL FOIL & POWDER Co., Ltd.) and K-0082P (METALOR) were used. As the solvent, tributyrin (boiling point 305° C., Wako Pure Chemical Industries, Ltd.), butyl stearate (boiling point 343° C., Wako Pure Chemical Industries, Ltd.), and stearic acid (boiling point 376° C., Wako Pure Chemical Industries, Ltd.) were used. The silver particles and the solvent were kneaded for 15 minutes with a stone mill at the blending ratio shown in Table 1 to manufacture a silver paste composition. The properties of this silver paste composition were measured to obtain the result shown in Table 1.

+ Open protocol
+ Expand
5

Silver Paste Composition Preparation

Check if the same lab product or an alternative is used in the 5 most similar protocols

Example 2

As the silver particles, AgC239 (FUKUDA METAL FOIL & POWDER Co., Ltd.) and K-0082P (METALOR) were used. As the solvent, tributyrin (boiling point 305° C., Wako Pure Chemical Industries, Ltd.) and stearic acid (boiling point 376° C., Wako Pure Chemical Industries, Ltd.) were used. The silver particles and the solvent were kneaded for 15 minutes with a stone mill at the blending ratio shown in Table 1 to manufacture a silver paste composition. The properties of this silver paste composition were measured to obtain the result shown in Table 1.

+ Open protocol
+ Expand

About PubCompare

Our mission is to provide scientists with the largest repository of trustworthy protocols and intelligent analytical tools, thereby offering them extensive information to design robust protocols aimed at minimizing the risk of failures.

We believe that the most crucial aspect is to grant scientists access to a wide range of reliable sources and new useful tools that surpass human capabilities.

However, we trust in allowing scientists to determine how to construct their own protocols based on this information, as they are the experts in their field.

Ready to get started?

Sign up for free.
Registration takes 20 seconds.
Available from any computer
No download required

Sign up now

Revolutionizing how scientists
search and build protocols!