Example 11

A 100 mL amber glass vial was placed into a glass drying oven at 120° C. to remove the absorbed water. This vial was then charged with 20 mL of zirconium(IV) n-propoxide and between 4 mL and 10 mL of acetyl acetone, with stirring. An exothermic reaction takes place to yield a zirconium (IV) (isopropoxide)n(acetyl acetonate)m sol-gel precursor. A sol-gel precursor that gave favorable results was zirconium (IV) (isopropoxide)2.6(acetyl acetonate)1.4, which was soluble within NMP.