Example 1

The respective ingredients shown in Table 1 were used and added to a beaker such that blending ratios are 29.97% of a sulfur-containing ester compound (A-1a), 0.03% of a sulfur-containing ester compound (A-1b), 45% of a modified silicone (C-1), and 25% of a surfactant (L-1). These were mixed well by stirring. While continuing to stir, ion exchanged water was added gradually to achieve a solids concentration of 25% and thereby prepare a 25% aqueous liquid of a carbon fiber precursor treatment agent of Example 1.