Example 1
In the Bioceramic compositions 1 and 2 as described in Table 1, the solid components were firstly prepared in powder form using a planetary mixer in the following sequence: sorosilicate, radiopacifying agent and setting agent at speed below 400 rpm, about 30 minutes until complete homogenization. The aqueous liquid carrier was prepared using a mechanical stirrer and the components were added in the following sequence: water, accelerator agent and plasticizer at speed below 800 rpm, about 60 minutes until complete homogenization.