Example 2
In Example 2, the potassium water glass used for references M1 and M2 was co-ground with the blast furnace slag used for references M1 and M2 for two minutes using a planetary ball mill. The obtained co-ground powder was then used in the formulations M1a and M2a shown in Table 2.
The resistances are shown in Table 3. Particularly, the resistances in NaOH significantly increased from 11% (M1) to 90% (M1a), as well as from 13% (M2) to 96% (M2a).